Ti/Fe ratio determines the overall Fischer-Tropsch performance of Fe-based bulk systems. Fe2TiO5 mediates iron reduction/carburization rate and minimizes oxidation of iron carbides under syngas conditions. Stable and active Fischer-Tropsch performance is achieved for Ti/Fe 0.48.