The microstructure characteristics in the ausformed Co consist of slender laths (γ phase) and blocky laths (ε phase). Strain-induced phase transformation occurs in ausformed Co after annealing treatment. The great improvement in hardness of the ausformed Co is ascribed to the very fine slender laths.