WO3-reduced graphene oxide (rGO) composite powders are prepared by spray pyrolysis process.
Ultrafine WO3 nanocrystals below 10 nm in size are dispersed within the rGO matrix.
Discharge capacity of the WO3-rGO composite powders at the 300th cycle is 546 mA h g−1.