Improvement of oxidation resistance of 9 mass% chromium steel for advanced-ultra supercritical power plant boilers by pre-oxidation treatment
详细信息    查看全文
文摘
Pre-oxidation treatment in argon gas containing 0.1 ppm to 1 volume % oxygen improves oxidation resistance of 9 mass% Cr steel in steam at 650 °C. A thin scale of Cr2O3-rich oxides is formed on the surface of 9Cr steel by the pre-oxidation treatment.The addition of Si enhances the formation of Cr2O3-rich oxide scale.