Dynamic recrystallization behavior and hot workability of AZ41M magnesium alloy during hot deformation
详细信息    查看全文
文摘

DRX mechanism is the dominant softening mechanism of AZ41M magnesium alloy during hot deformation.

The DRX kinetic model can be expressed as: View the MathML source.

The optimum hot working parameters are the temperature range of 390–450 °C and strain rate range of 0.005–0.015 s−1.