Enhancing phase-transition sensitivity of tungsten-doped vanadium dioxide by high-temperature annealing
详细信息    查看全文
文摘

W-doped V2O5 was obtained by a molten and water quenching technology.

W doped VO2 was synthesized by a facile solid reaction.

The effects of thermal treatment for W doped VO2 were studied detailedly.

High temperature annealing could remarkably enhance the MIT sensitivity of VO2.

Electrical resistance is simultaneously sensitive in the phase transition.