Carbonate co-precipitation synthesis of Er3+:Lu2O3 nanopowders.
Pure-phase crystalline Lu2O3 was completely formed at 800 °C.
The ceramic sample showed a visually dominant green UCL under 980 nm excitation.
The UCL of the Er3+:Lu2O3 transparent ceramics suggests a two-photon process.