A low-loss tellurite step-index optical fiber was made by the suction casting and rod in tube methods.
The zero-dispersion wavelength of the fiber is close to that of the material.
The FWM-based wavelength conversion was performed by using a 1-m-long fiber. Its wavelength spacing can be as broad as 966 nm.