文摘
Novel microporous beads with the particle size of about 90μm were prepared, for the first time, from cellulose and konjac glucomannan (RC/KGM3) in 1.5M NaOH/0.65M thiourea aqueous solution by emulsification method. The microporous beads were then modified with silane to avoid the adsorption of polymers containing hydroxyl groups, coded as RC/KGM3-Si. A preparative size-exclusion chromatographic (SEC) column (500mm×20mm) was packed with RC/KGM3-Si, and its exclusion limit and fractionation range of the stationary phase were, respectively, weight-average molecular masses (Mw) of 4.8×l05g/mol and 5.3×l03–4.8×l05g/mol for polystyrene in tetrahydrofuran. The preparative SEC column was used to fractionate poly(?-caprolactone) (PCL, Mw