Simultaneously feeding TC17 wire and Stellite 20–Si3N4–TiC–Sb mixed powders formed composites.
Sb addition in laser molten pool was favorable to the formations of UNs.
UNs were intertwined with amorphous, leading the yarn-shape materials to be produced.
Ti entered into molten pool from the wire and TA1, which may react with Si or N.