Investigation of (WAl)C-Co ceramic composites with the additions of fluoride solid lubricants: Preparation, mechanical properties and tribological behaviors
详细信息    查看全文
文摘
(WAl)C-Co/fluoride (CaF2, BaF2, CaF2/BaF2) self-lubricating ceramic composites prepared by mechanical alloying and hot pressing sintering was reported for the first time. The influence of the fluorides on the mechanical properties, friction coefficient and wear rate of the composites was also evaluated. The friction coefficient of the (W0.67Al0.33)C0.67-Co/fluoride materials is in the range of 0.22-0.36, with the wear rate in the order of 10? 6 mm3 N? 1 m? 1. The fluoride in the (W0.67Al0.33)C0.67-Co/fluoride plays a key role in decreasing the friction coefficient and wear rate. The wear layer formed during friction process exerts a significant influence on the tribological properties, which would increase the friction coefficient but protect the worn surface.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700