We successful synthesized xonotlite fiber from carbide slag and acid residues.
We find an effective way to deal with millions of tons of solid waste.
Much longer xonotlite fibers (10–15 μm) were obtained by rapid synthesis.
The transition steps is C–S–H block, tobermorite needle, and then xonotlite fiber.