Effect of ZnO level in secondary copper smelting slags on slag/magnesia-chromite refractory interactions
详细信息    查看全文
文摘
To determine the effect of ZnO in ZnO-containing fayalite (ZFS) slags on the degradation of magnesia-chromite refractories, the corrosion behaviour of a direct-bonded magnesia-chromite refractory was studied by rotating refractory finger tests at 1200 °C under reducing atmosphere. In addition, MgO crucible tests at these conditions were performed to investigate in particular the effect of ZnO on the slag/MgO interaction. The dissolution of MgO from periclase into the ZFS slags is not enhanced by increasing the ZnO content in the slags. (Fe,Mg,Zn)2SiO4 olivine and (Fe,Mg,Zn)O solid solution are the only two products in the slag/MgO interfacial reactions, even when the ZnO content in the ZFS slag reaches 16.7 wt%. The diffusion of ZnO into the chromite grains to form the (Fe,Mg,Zn)(Fe,Al,Cr)2O4 spinel was favoured with increasing the ZnO content in ZFS slags.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700