Platinum-decorated Cu(InGa)Se2/CdS photocathodes: Optimization of Pt electrodeposition time and pH level
详细信息    查看全文
文摘
class="listitem" id="list_ulist0010">
class="label">•

The CIGS/CdS layers were electrodeposited with Pt using various deposition times.

class="label">•

The Pt electrodeposition time of 20 min yielded −24.16 mA/cm2 at optimum.

class="label">•

The effect of the pH on the PEC performance was investigated.