Al86Ni6Y4.5La1.5Co2 splats were produced by rapid quenching in a splat quencher.
The texture was analyzed by X-ray diffraction and Rietveld analysis.
No texture was observed in the as quenched specimens.
(110) texture evolved after annealing cold rolled splats to 360 °C.
(110) texture is ascribed to stress fields induced by the shear bands.