An efficient milling-assisted technology to use K-feldspar and mineralize CO2.

Facilitation the potassium extraction under mild conditions (e.g. 30–40 °C).

A maximum potassium extraction ratio of ∼80% and CO2 mineralization ratio of ∼5%.

Fragmentation, amorphization and lattice distortion enhance reaction activities.