The properties of mortar used heavy weight waste glass as fine aggregate were compared.
Unit volume weight and shielding performance increased with the content of waste glass.
However, the strength decreased as the waste glass substitution increased.
The waste glass substitution affected on pores ranging from 10–100 nm.