4H-SiC epilayers grown by standard and chlorinated chemistry were analyzed for their minority carrier lifetime and deep level recombination centers using time-resolved photoluminescence (TRPL) and standard deep level transient spectroscopy (DLTS). Next to the well-known Z1/2 deep level a second effective lifetime killer, RB1 (activation energy 1.05 eV, electron capture cross section 2 脳 10鈥?6 cm2, suggested hole capture cross section (5 卤 2) 脳 10鈥?5 cm2), is detected in chloride chemistry grown epilayers. Junction-DLTS and bulk recombination simulations are used to confirm the lifetime killing properties of this level. The measured RB1 concentration appears to be a function of the iron-related Fe1 level concentration, which is unintentionally introduced via the corrosion of reactor steel parts by the chlorinated chemistry. Reactor design and the growth zone temperature profile are thought to enable the formation of RB1 in the presence of iron contamination under conditions otherwise optimal for growth of material with very low Z1/2 concentrations. The RB1 defect is either an intrinsic defect similar to RD1/2 or EH5 or a complex involving iron. Control of these corrosion issues allows the growth of material at a high growth rate and with high minority carrier lifetime based on Z1/2 as the only bulk recombination center.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700