Interfacial Free Energy Driven Nanophase Separation in Poly(3-hexylthiophene)/[6,6]-Phenyl-C61-butyric Acid Methyl Ester Thin Films
详细信息    查看全文
文摘
The nanostructure of thermally annealed thin films of poly(3-hexylthiophene) (P3HT) and [6,6]-phenyl-C61-butyric acid methyl ester (PCBM) blends on hydrophobic and hydrophilic substrates was studied to unravel the relationship between the substrate properties and the phase structure of polymer blends in confined geometry. Indeed, the nature of the employed substrates was found to affect the extent of phase separation, the PCBM aggregation state and the texture of the whole system. In particular, annealing below the melting temperature of the polymer yielded the formation of PCBM nanometric crystallites on the hydrophobic substrates, while mostly amorphous microscopic aggregates were formed on the hydrophilic ones. Moreover, while an enhanced in-plane orientation of P3HT lamellae was promoted on hydrophobic substrates, a markedly tilted geometry was produced on the hydrophilic ones. The observed effects were interpreted in terms of a simple model connecting the interface free energy for the blend films to the different polymer chain mobility and diffusion velocity of PCBM molecules on the different substrates.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700