Mercury Oxidation over the V2O5(WO3)/TiO2 Commercial SCR Catalyst
详细信息    查看全文
文摘
Mercury oxidation by hydrochloric acid over the V2O5(WO3)/TiO2 commercial SCR catalyst was investigated. Both fresh and aged catalysts with honeycomb structure, which were exposed to a coal combustion flue gas in a coal-fired boiler for over 71 000 h, were examined. The aged catalysts were characterized by X-ray and SEM-EDX analysis to examine the presence of ash deposition on the surface. The mercury oxidation rate was enhanced by increasing HCl concentrations and inhibited strongly by the presence of NH3. This behavior could be explained by a kinetic model assuming that HCl competes for the catalyst active sites against NH3. As the catalyst operation time increased, the mercury oxidation rate was observed to decrease considerably in the presence of NH3 while NO reduction rate was apparently nearly unchanged. By examining aged catalysts, deposits stemming from fly ash and SO2/SO3 were observed to accumulate continuously on the catalyst surface. The ash deposited on the surface may partially block the active catalyst sites and decrease their number. The decrease of the number of active sites on the catalyst surface caused NH3 to remain unreacted in the honeycomb catalyst. The decrease of the Hg0 oxidation rate was caused by the inhibition effect of NH3 remaining in the catalyst.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700