详细信息    查看全文
  • 作者:Jinkai Xu ; Linshuai Zhang ; Huadong Yu…
  • 关键词:WEDM ; HS ; Ti ; 6Al ; 4V ; Surface ; Coloring ; Microstructure ; Antifriction properties
  • 刊名:The International Journal of Advanced Manufacturing Technology
  • 出版年:2015
  • 出版时间:March 2015
  • 年:2015
  • 卷:77
  • 期:1-4
  • 页码:729-734
  • 全文大小:815 KB
  • 参考文献:1. Delplancke, JL, Degrez, M, Fontana, A, Winand, R (1982) Self-colour anodizing of titanium. Surf Technol 16: pp. 153-162 CrossRef
    2. Jiang, W, Shen, DX, Zhang, YK, Zhang, ZY, Wang, SC, Zhang, YH, Han, YC, Ren, WM (2005) Study on coloring technology of titanium alloy. Mater Protect 38: pp. 12-14
    3. Pérez del Pino, A, Serra, P, Morenza, JL (2002) Oxidation of titanium through Nd:YAG laser irradiation. Appl Surf Sci 197: pp. 887-890 CrossRef
    4. Pérez del Pino, A, Serra, P, Morenza, JL (2002) Coloring of titanium by pulsed laser processing in air. Thin Solid Films 415: pp. 201-205 CrossRef
    5. Ohmori, H, Katahira, K, Mizutani, M, Komotori, J (2004) Investigation on color-finishing process conditions for titanium alloy applying a new electrical grinding process. CIRP Ann-Manuf Technol 53: pp. 455-458 CrossRef
    6. Peng, WW, Zeng, WD, Zhang, YW, Shi, CL, Quan, B, Wu, JD (2013) The effect of colored titanium oxides on the color change on the surface of Ti-5Al-5Mo-5V-1Cr-1Fe alloy. JMEPEG 22: pp. 2588-2593 CrossRef
    7. Garg, RK, Singh, KK, Sachdeva, A, Sharma, VS, Ojha, K, Singh, S (2010) Review of research work in sinking EDM and WEDM on metal matrix composite materials. Int J Adv Manuf Technol 50: pp. 611-624 CrossRef
    8. Han, FZ, Chang, G, Feng, ZJ, Isago, S (2009) Measurement of wire electrode temperature in WEDM. Int J Adv Manuf Technol 41: pp. 871-879 CrossRef
    9. Zhao, WS (2003) Advanced electrical discharge machining technology. National Defence Industry Press, Beijing
    10. Wang, AC, Yan, BH, Tang, YX, Huang, FY (2005) The feasibility study on a fabricated micro slit die using micro EDM. Int J Adv Manuf Technol 25: pp. 10-15 CrossRef
    11. Gao, SC, Li, YH, Zhang, LN, Wan, ZL (2012) Characterization and electrochemistry analysis of colored films on the surface of TA2 pure titanium by anodic oxidation using phosphate acid. Rare Met Mat Eng 41: pp. 1049-1054
    12. Yan, X, Zhang, QY, Lu, JH, Zhao, W (2004) Recentprogress in preparation and application for iridium/oxide films. Rare Met 28: pp. 757
    13. Tsai, YY, Song, PL, Jeffrey Shih, CF (2013) Colorful oxide film formation on titanium by using EDM process. Int J Precis Eng Man 14: pp. 1933-1937 CrossRef
    14. Yu, DY, Tan, HY (2006) Engineering Optics, M. Mechanical Industry Press, Beijing
    15. Woo, YM, Yeo, SH, Tan, PC (2013) Critical wall thickness in electrical discharge machining. Int J Adv Manuf Technol 64: pp. 821-828 CrossRef
    16. Zhang, YK, Wang, SC, Guo, J (2004) Effect of hydrogen oxygen on performance properties and surface quality of Ti-6Al-4V alloy. Changchun Univ Sci Technol 3: pp. 87-88
  • 刊物类别:Engineering
  • 刊物主题:Industrial and Production Engineering
    Production and Logistics
    Mechanical Engineering
    Computer-Aided Engineering and Design
  • 出版者:Springer London
  • ISSN:1433-3015
文摘
In this paper, the technology of high-speed wire electrical discharge machining (WEDM-HS) is used for coloring the surface of Ti-6Al-4V alloy, and the antifriction properties of Ti-6Al-4V alloy-colored surface are analyzed. For this paper, we have prepared six kinds of tone by adjusting the electrical discharge processing parameters on the surface of Ti-6Al-4V alloy. Using laser confocal microscopy that observed the microstructure morphology of reaction film after the 1000-h sunlight and water immersion aimed at the coloring mechanism of Ti-6Al-4V alloy surface. RETC micro-friction and wear tester were used to analyze the friction properties of the colored surface with dry friction conditions. The experimental results show that the colored surface after WEDM-HS processing has good stability and durability. Moreover, the average friction coefficient is reduced by 200?% compared with the unprocessed surface, showing excellent antifriction performance.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700