High-Temperature Scale Formation of Fe–36 % Ni Bicrystals in Air
详细信息    查看全文
文摘
Fe–36 % Ni bicrystals were oxidized at temperatures from 1100 to 1250 K in air, both under and without tensile stress. The scales were divided into three categories: external scales, intragranular subscales, and intergranular subscales. A linear relationship exists beween the thickness of scales and subscales and the square root of oxidation time. Tensile stress significantly accelerates intergranular oxidation, but has essentially no influence on either the formation of intragranular subscales or that of external scales. The external scales are composed of α-Fe2O3 and Fe3O4 after a longer oxidation time. The intergranular and intragranular subscales consist of Fe3O4 and FeO particles and an Ni-enriched matrix. Cellular or dendritic oxide nodules sometimes exist in the intragranular subscales, causing their frontier interfaces to significantly undulate.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700