Preparation of Palladium Supported on Ferric Oxide Nano-catalysts for Carbon Monoxide Oxidation in Low Temperature
详细信息    查看全文
  • 作者:Fagen Wang ; Yan Xu ; Kunfeng Zhao ; Dannong He
  • 关键词:Pd/Fe2O3 ; Carbon monoxide ; Catalytic oxidation ; Low temperature
  • 刊名:Nano-Micro Letters
  • 出版年:2014
  • 出版时间:July 2014
  • 年:2014
  • 卷:6
  • 期:3
  • 页码:233-241
  • 全文大小:466KB
  • 参考文献:[1]K. N. Rao, P. Bharali, G. Thrimurthulu and B. M. Reddy, 鈥淪upported Copper-ceria catalysts for low temperature CO oxidation鈥? Catal. Commun. 11(10), 863鈥?66 (2010). http://鈥媎x.鈥媎oi.鈥媜rg /10.1016/j.catcom.2010.03.009CrossRef
    [2]D. Gamarra, C. Belver, M. Garcia, and A. Arias, 鈥淪elective CO oxidation in excess H2 over copper-ceria catalysts: identification of active entities/species鈥? J. Am. Chem. Soc. 129(40), 12064鈥?2065 (2007). http://鈥媎x.鈥媎oi.鈥媜rg /10.1021/ja073926gCrossRef
    [3]W. Xie, Y. Li, Z. Liu, M. Haruta and W. Shen, 鈥淟owtemperature oxidation of CO catalysed by Co3O4 nanorods鈥? Nature 458(7239), 746鈥?49 (2009). http://鈥媎x.鈥媎oi.鈥媜rg /10.1038/nature07877CrossRef
    [4]K. Zhao, B. Qiao, J. Wang, Y. Zhang and T. Zhang, 鈥淎 highly active and sintering-resistant Au/FeOx鈭?/sub> hydroxyapatite catalyst for CO oxidation鈥? Chem. Commun., 47(6), 1779鈥?781 (2011). http://鈥媎x.鈥媎oi.鈥媜rg /10.1039/C0CC04171HCrossRef
    [5]S. Li, G. Liu, H. Lian, M. Jia, G. Zhao, D. Jiang and W. Zhang, 鈥淟ow-temperature CO oxidation over supported Pt catalysts prepared by colloid-deposition method鈥? Catal. Commun. 9(6), 1045鈥?049 (2008). http://鈥媎x.鈥媎oi.鈥媜rg /10.1016/j.catcom.2007.10.016CrossRef
    [6]A. Satsuma, K. Osaki, M. Yanagihara, J. Ohyama and K. Shimizu, 鈥淎ctivity controlling factors for low-temperature oxidation of CO over supported Pd catalysts鈥? Appl. Catal. B: Environ. 132鈥?33, 511鈥?18 (2013).http://鈥媎x.鈥媎oi.鈥媜rg /10.1016/j.apcatb.2012.12.025CrossRef
    [7]M. Haruta, 鈥淕old as a novel catalyst in the 21st century: Preparation, working mechanism and applications鈥? Gold Bull. 37(1鈥?), 27鈥?6 (2004). http://鈥媎x.鈥媎oi.鈥媜rg /10.1007/BF03215514CrossRef
    [8]J. Moghaddam, S. Mollaesmail and S. Karimi, 鈥淭he Influence of Morphology on Photo-catalytic Activity and Optical Properties of Nano-crystalline ZnO Powder鈥? Nano-Micro Letters. 4(4), 197鈥?01 (2012). http://鈥媎x.鈥媎oi.鈥媜rg /10.3786/nml.v4i4.p197-201CrossRef
    [9]M. A. Bollinger and M. A. Vannice, 鈥淎 kinetic and DRIFT study of low temperature carbon monoxide over Au-TiO2 catalysts鈥? Appl. Catal. B: Environ. 8(4), 417鈥?43 (1996). http://鈥媎x.鈥媎oi.鈥媜rg /10.1016/0926-3373(96)90129-0
    [10]G. Y. Wang, H. L. Lian, W. X. Zhang, D. Z. Jiang and T. H. Wu, 鈥淪tability and deactivation of Au/Fe2O3 catalysts for CO oxidation at ambient temperature and moisture鈥? Kin. Catal. 43(3), 433鈥?42 (2002). http://鈥媎x.鈥媎oi.鈥媜rg /10.1023/A:1016026405985CrossRef
    [11]M. Dateand M. Haruta, 鈥淢oisture effect on CO oxidation over Au/TiO2 catalyst鈥? J. Catal. 201(2), 221鈥?24 (2001). http://鈥媎x.鈥媎oi.鈥媜rg /10.1006/jcat.2001.3254CrossRef
    [12]M. Jin, J. Park, J. Shon, Z. Li, Y. Park and J. Kim, 鈥淟ow temperature CO oxidation over Pd catalysts supported on highly ordered mesoporous metal oxides鈥? Catal. Today 185(1), 183鈥?90 (2012). http://鈥媎x.鈥媎oi.鈥媜rg /10.1016/j.cattod.2011.09.019CrossRef
    [13]F. Liang, H. Zhu, Z. Qin, G. Wang and J. Wang, 鈥淓ffects of CO2 on the stability of Pd/CeO2TiO2 catalyst for low-temperature CO oxidation鈥? Catal. Commun. 10(5), 737鈥?40 (2009). http://鈥媎x.鈥媎oi.鈥媜rg /10.1016/j.catcom.2008.11.031CrossRef
    [14]B. Qiao, L. Liu, J. Zhang and Y. Deng, 鈥淧reparation of highly effective ferric hydroxide supported noble metal catalysts for CO oxidations: From gold to palladium鈥? J. Catal. 261(2), 241鈥?44 (2009). http://鈥媎x.鈥媎oi.鈥媜rg /10.1016/j.jcat.2008.11.012CrossRef
    [15]S. Bernal, J. J. Calvino, M. A. Cauqui, J. M. Gatica, C. Larese, J. A. P. Omil and J. M. Pintado, 鈥淪ome recent results on metal/support interaction effects in NM/CeO2 (NM: noble metal) catalysts鈥? Catal. Today 50(2), 175鈥?06 (1999). http://鈥媎x.鈥媎oi.鈥媜rg /10.1016/S0920-5861(98)00503-3CrossRef
    [16]B. Qiao, A. Wang, X. Yang, L. F. Allard, Z. Jiang, Y. Cui, J. Liu, J. Li and T. Zhang, 鈥淪ingle-atom catalysis of CO oxidation using Pt1/FeOx鈥? Nature Chem. 3(8), 634鈥?41 (2011). http://鈥媎x.鈥媎oi.鈥媜rg /10.1038/nchem.1095CrossRef
    [17]L. Liu, F. Zhou, L. Wang, X. Qi, F. Shi and Y. Deng, 鈥淟ow-temperature CO oxidation over supported Pt, Pd catalysts: Particular role of FeOx support for oxygen supply during reactions鈥? J. Catal. 274(1), 1鈥?0 (2010). http://鈥媎x.鈥媎oi.鈥媜rg /10.1016/j.jcat.2010.05.022CrossRef
    [18]Q. Fu, W. Li, Y. Yao, H. Liu, H. Su, D. Ma, X. Gu, L. Chen, Z. Wang, H. Zhang, B. Wang and X. H. Bao, 鈥淚nterface-confined ferrous centers for catalytic oxidation鈥? Science 238(5982), 1141鈥?144 (2010). http://鈥媎x.鈥媎oi.鈥媜rg /10.1126/science.1188267CrossRef
    [19]L. Li, A. Wang, B. Qiao, J. Lin, Y. Huang, X. Wang and T. Zhang, 鈥淥rigin of the high activity of Au/FeOx for low-temperature CO oxidation: Direct evidence for a redox mechanism鈥? J. Catal. 299, 90鈥?00 (2013). http://鈥媎x.鈥媎oi.鈥媜rg /10.1016/j.jcat.2012.11.019CrossRef
    [20]L. Liu, B. Qiao, Y. He, F. Zhou, B. Yang and Y. Deng, 鈥淐atalytic co-oxidation of CO and H2 over FeOx-supported Pd catalyst at low temperatures鈥? J. Catal. 294, 29鈥?6 (2012). http://鈥媎x.鈥媎oi.鈥媜rg /10.1016/j.jcat.2012.06.018CrossRef
    [21]M. G. Musolino, C. Busacca, F. Mauriello and R. Pietropaolo, 鈥淎liphatic carbonyl reduction promoted by palladium catalysts under mild conditions鈥? Appl. Catal. A: Gen. 379(1鈥?), 77鈥?6 (2010). http://鈥媎x.鈥媎oi.鈥媜rg /10.1016/j.apcata.2010.03.008CrossRef
    [22]J. Jia, J. Shen, L. Lin, Z. Xu, T. Zhang and D. Liang, 鈥淎 study on reduction behaviors of the supported platinumiron catalysts鈥? J. Mol. Catal. A: Chem. 138(2鈥?), 177鈥?84 (1999). http://鈥媎x.鈥媎oi.鈥媜rg /10.1016/S1381-1169(98)00147-2CrossRef
    [23]W. C. Conner and J. L. Falconer, 鈥淪pillover in Heterogeneous Catalysis鈥? Chem. Rev. 95(3), 759鈥?88 (1995). http://鈥媎x.鈥媎oi.鈥媜rg /10.1021/cr00035a014CrossRef
    [24]X. Mou, B. Zhang, Y. Li, L. Yao, X. Wei, D. S. Su and W. Shen, 鈥淩od-Shaped Fe2O3 as an Efficient Catalyst for the Selective Reduction of Nitrogen Oxide by Ammonia鈥? Angew. Chem. Int. Ed. 51(12), 2989鈥?993 (2012). http://鈥媎x.鈥媎oi.鈥媜rg /10.1002/anie.201107113CrossRef
    [25]S. H. Oh and G. B. Hoflund, 鈥淟ow-temperature catalytic carbon monoxide oxidation over hydrous and anhydrous palladium oxide powders鈥? J. Catal. 245(1), 35鈥?4 (2007). http://鈥媎x.鈥媎oi.鈥媜rg /10.1016/j.jcat.2006.09.016CrossRef
    [26]M. Jin, J. N. Park, J. K. Shon, J. H. Kim, Z. Li, Y. K. Park and J. M. Kim, 鈥淟ow temperature CO oxidation over Pd catalysts supported on highly ordered mesoporous metal oxides鈥? Catal. Today 185(1), 183鈥?90 (2012). http://鈥媎x.鈥媎oi.鈥媜rg /10.1016/j.cattod.2011.09.019CrossRef
    [27]S. Y. Christou and A. M. Efstathiou, 鈥淓ffects of Pd Particle Size on the Rates of Oxygen Back-Spillover and CO Oxidation under Dynamic Oxygen Storage and Release Measurements over Pd/CeO2 Catalysts鈥? Top Catal. 42鈥?3(1鈥?), 351鈥?55 (2007). http://鈥媎x.鈥媎oi.鈥媜rg /10.1007/s11244-007-0204-0CrossRef
    [28]J. C. F. Gonzalez, V. A. Bhirud and B. C. Gates, 鈥淎 highly active catalyst for CO oxidation at 298 K: mononuclear AuIII complexes anchored to La2O3 nanoparticles鈥? Chem. Commun. 5275鈥?277 (2005). http://鈥媎x.鈥媎oi.鈥媜rg /10.1039/b509629d
    [29]T. Na, F. Wang, H. Li and W. Shen, 鈥淚nfluence of Au particle size on Au/CeO2 catalysts for CO oxidation鈥? Catal. Today 175(1), 541鈥?45 (2011). http://鈥媎x.鈥媎oi.鈥媜rg /10.1016/j.cattod.2011.04.027CrossRef
    [30]N. W. Cant, P. C. Hicks and B. S. Lennon, 鈥淪teadystate oxidation of carbon monoxide over supported noble metals with particular reference to platinum鈥? J. Catal. 54(3), 372鈥?83 (1978). http://鈥媎x.鈥媎oi.鈥媜rg /10.1016/0021-9517(78)90085-4CrossRef
    [31]I. Stara, V. Nehasil and V. Matolin, 鈥淭he influence of particle size on CO oxidation on Pd/alumina model catalyst鈥? Surf. Sci. 331鈥?33, 173鈥?77 (1995). http://鈥媎x.鈥媎oi.鈥媜rg /10.1016/0039-6028(95)00183-2CrossRef
    [32]F. Boccuzzi, A. Chiorino, S. Tsubota and M. Haruta, 鈥淔TIR study of carbon monoxide and scrambling at room temperature over gold supported on ZnO and TiO2鈥? J. Phys. Chem. 100(9), 3625鈥?631 (1996). http://鈥媎x.鈥媎oi.鈥媜rg /10.1021/jp952259nCrossRef
    [33]T. Shido and Y. Iwasawa, 鈥淩eactant-promoted reaction mechanism for water-gas shift reaction on Rhdoped CeO2鈥? J. Catal. 141(1), 71鈥?1 (1993). http://鈥媎x.鈥媎oi.鈥媜rg /10.1006/jcat.1993.1119CrossRef
    [34]B. Chang, B. W. Jang, S. Dai and S. H. Overbury, 鈥淭ransient studies of the mechanism of CO oxidation over Au/TiO2 using time-resolved FTIR spectroscopy and product analysis鈥? J. Catal. 236(2), 392鈥?00 (2005). http://鈥媎x.鈥媎oi.鈥媜rg /10.1016/j.jcat.2005.10.006CrossRef
    [35]Y. Shen, Y. Guo, L. Wang, Y. Wang, Y. Guo, X. Gong and G. Lu, 鈥淭he stability and deactivation of Pd-Cu- Clx/Al2O3 catalyst for low temperature CO oxidation: an effect of moisture鈥? Catal. Sci. Techno. 1, 1202鈥?207 (2011). http://鈥媎x.鈥媎oi.鈥媜rg /10.1039/c1cy00146aCrossRef
  • 作者单位:Fagen Wang (15)
    Yan Xu (15)
    Kunfeng Zhao (15)
    Dannong He (15)

    15. National Engineering Research Center for Nanotechnology, Shanghai, 200241, China
  • 刊物类别:Nanotechnology and Microengineering; Nanotechnology; Nanoscale Science and Technology;
  • 刊物主题:Nanotechnology and Microengineering; Nanotechnology; Nanoscale Science and Technology;
  • 出版者:Springer Berlin Heidelberg
  • ISSN:2150-5551
文摘
Catalytic property of Pd/Fe2O3 catalysts on carbon monoxide (CO) oxidation at low temperature were investigated in this paper. Both the as-prepared and H2-pretreated Pd/Fe2O3 catalysts show catalytic performances on CO oxidation. The CO was completely converted at 333 K for the as-prepared sample, whereas at 313 K for H2-pretreated Pd/Fe2O3-573 catalyst. The catalytic performance of the Pd/Fe2O3 catalyst decreases with increased calcination temperature. This may be due to the increased crystallinity of the support and decreased metal-support interaction. Progressive deactivation of the catalysts during long-time reaction was associated with the formation of carbonates on the catalyst surface that inhibits CO activation or intermediate transformation. Keywords Pd/Fe2O3 Carbon monoxide Catalytic oxidation Low temperature

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700