Damages on steel surface at the incubation stage of the vibration cavitation erosion in water
详细信息查看全文 | 推荐本文 |
摘要
To investigate the damage mechanism of the cavitation erosion at the incubation stage, a kind of polished 40Cr steel was used as the sample in the vibration cavitation erosion experiment. After 1-min experiment, three kinds of erosion pits were found on the sample surface, they are complete pits, incomplete pits and thermal pits in this paper. Numerical simulation of a bubble collapse process in Fluent environment explains the formations of the three kinds of erosion pits. The micro-jet with a strong radius flow around is the main reason for the complete pits and their step-like openings, the shock wave generated outside the jet function domain is the main reason for the incomplete pit, and the high temperature in the compressed bubble at the moment of collapse is considered as the reason for the formation of the thermal pits.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700