A dense SiC/Ti3Si(Al)C2 composite was synthesized by in situ hot pressing powders of Si, TiC and Al as a sintering additive at 1500 掳C for 2 h under 30 MPa in Ar atmosphere. This composite has a fine-grained and homogeneous microstructure with grain sizes of 5 渭m for Ti3Si(Al)C2 and of 1 渭m for SiC. The SiC/Ti3Si(Al)C2 composite possesses an improved oxidation resistance, with parabolic rate constants of 4.57 脳 10鈭? kg2/m4/s at 1200 掳C and 1.31 脳 10鈭? kg2/m4/s at 1300 掳C. This study provides an experimental evidence to confirm the formation of amorphous phases in the oxide scale of the SiC/Ti3Si(Al)C2 composite. Microstructure and phase composition of the SiC/Ti3Si(Al)C2 composite and oxide scales were identified by X-ray diffractometry and scanning electron microscopy. The mechanism for the enhanced oxidation resistance has been discussed.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700