The regeneration of W and Mo supported on γ and α–θAl2O3 catalysts used during 1-butene skeletal isomerization, was studied. The regenerated catalysts were characterized by several techniques and the results compared with those of the fresh catalysts. It was found that it is necessary a 15 h at 465 °C treatment to completely eliminate coke on W/γA and Mo/γA, both catalysts recovering the initial activity and selectivity. Using this procedure, the properties of the catalysts were not modified. The same treatment did not allow the activity recovery in W/α–θA, due to differences in the nature of coke, that is aromatic or pregraphitic, and could not be totally removed.