Influence of additions of coal fly ash and quartz on hydrothermal solidification of blast furnace slag
详细信息查看全文 | 推荐本文 |
摘要
Blast furnace water-cooled slag (BFWS) has been solidified hydrothermally with tobermorite formation. The experimental results showed that the addition of fly ash and quartz was favorable to the formation of tobermorite, and the strength development of solidified body depended on both of the tobermorite formation and filling degree of formed tobermorite in the spaces between BFWS particles. The fly ash added appeared to have a higher reactivity than the quartz used during the initial hydrothermal processing due to the higher solubility of glassy phase in fly ash. The tobermorite formation seemed to be very sensitive to the fly ash content, e.g., the addition of fly ash 10–20 mass%was favorable to tobermorite formation, while the excessive addition of fly ash (> 20 mass%) appeared to impede the tobermorite formation. The excessive addition of quartz was also shown to exert a negative effect on the tobermorite formation, which causes strength deduction.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700