Contribution of Pendant Ester Group Hydrolysis to the Erosion of Acrylic Polymers in Binders Aimed at Organotin-Free Antifouling Paints
详细信息
下载全文
推荐本文 |
摘要
Specific polymeric material applications as bioactive molecules delivery systems involve a strictly controlled degradation of polymer matrixes. One possibility to obtain a zero-order kinetic for small molecules release consists in a simple hydrolysis of ester groups contained in the macromolecular structure. The chemical degradation can lead to the continuous surface erosion of the formulated resins without loss of their mechanical properties and to a permanent activity of the delivery systems. Hydrolysis is a very well-known reaction in the case of organic molecules containing ester groups. The mechanism seems to be more complicated when ester groups are located in macromolecular structures. With the aim of antifouling applications, acrylic acid polymers bearing lateral ester groups of different chemical structures (hydrophilic, hydrophobic, hydrolyzable) have been prepared, characterized, and immersed in water, at pH 8, and their hydrolysis has been studied. Experimental data display two parameters, at least, which must be taken into account: the reactivity of the ester groups toward hydrolysis and the hydrophilic/hydrophobic balance of the polymer. The susceptibility of the acrylic polymers to hydrolysis has been compared to the erosion characteristics of the corresponding films. The results confirm that hydrolysis is necessary to obtain a regular degradation of the films without loss of mechanical properties. A relationship has been observed between the characteristics of hydrolysis and erosion for each studied polymer.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700