摘要
本文介绍了安钢冷轧有限公司1 550mm酸连轧机组生产0.25~0.40mm厚度薄规格钢卷心形卷缺陷,通过带钢板形控制和卷取张力控制的优化,并对新型钢套筒不断进行试验,逐步实现了0.4mm以下厚度带钢不同厚度范围带钢的卷形控制。
Thispaperintroducedthedefectofcoronalcoilof 0.25~0.40 mmthingaugesteelcoilproducedby 1550 mm acid continuous rolling mill of Angang Cold Rolling Co., Ltd. Through optimization of strip shape control and coiling tension control, continuous test of new steel sleeve, the coiling control of strip with different thickness ranges of less than 0.4 mm thickness was gradually realized.