摘要
本文提出一种局部热平衡法计算干熄焦烧损率的方法,及利用碳平衡法反推干熄焦炉的空气泄漏量的方法。通过两种方法联立,成功计算出沙钢干熄焦焦炭的烧损率,以及整个系统中的空气泄漏量。根据烧损率原因,制定出循环气体管道补漏等措施,使干熄焦烧损率显著降低。
This paper present a kind of calculation methods of loss of ignition of dry quenched coke and air leakage. By two methods, loss of ignition of dry quenched coke and air leakage was calculated. According to the reason, measure of mending circulation gas pipe was implemented. Loss of ignition of dry quenched decreased remarkably.
引文
[1]高哲发,苏轮忠,卓昕.应用气体成分测算干熄焦系统中碳的烧损[J].燃料与化工,2010,41(3).37-40.
[2]朱志雄,李宁.干熄焦焦炭烧损率的控制[J].浙江冶金,2009,2:24-28.
[3]张素芬,向宇,张良.干熄焦焦炭烧损率的优化措施[J].河南冶金,2013,21(1):27-30.
[4]王伟民,刘杰,曹银平,等.干熄焦烧损率的统计方法及烧损率因素探讨[J].燃料与化工,2010,41(2):24-26.
[5]杨太宝,牛爱宁,李训智.150t/h干熄焦系统焦炭烧损率的控制[J].燃料与化工,2010,41(4):39-41.
[6]张涵,李剑利,曹文,等.安钢75t/h干熄焦物料与热量衡算及分析[J].广东化工,2010,37(208).109-110.