2.25Cr-1Mo-0.25V材质加氢钢性能不合原因分析及解决措施
详细信息    查看全文 | 推荐本文 |
  • 英文篇名:Cause Analysis and Solution of Performance Unqualification of 2. 25Cr-1Mo-0. 25V Steel for Hydrogenation Reactor Shell Forging
  • 作者:黄保国
  • 英文作者:Huang Baoguo;
  • 关键词:冲击不合格 ; 缺陷 ; 组织 ; 冷却速度
  • 英文关键词:unqualified impact properties;;defects;;microstructure;;cooling rate
  • 中文刊名:DXZL
  • 英文刊名:Heavy Castings and Forgings
  • 机构:中国一重集团有限公司;
  • 出版日期:2019-07-09
  • 出版单位:大型铸锻件
  • 年:2019
  • 期:No.190
  • 语种:中文;
  • 页:DXZL201904009
  • 页数:3
  • CN:04
  • ISSN:51-1396/TG
  • 分类号:27-29
摘要
承制的某加氢反应器筒节锻件在调质后出现批量性能不合格质量问题,通过缺陷分析,查找原因,并在后续生产中制定了有效预防措施,保证了后续生产加氢筒节全部一次调质合格。
        After quenching and tempering,the performance of a certain hydrogenation reactor shell forging in batch has been found to be unqualified. The reasons have been found through defect analysis,and effective preventive measures have been formulated to ensure that all the hydrogenation reactor shell forging in the subsequent production have been qualified after the first quenching and tempering.