摘要
以中海油SZ36-1减三线馏分油为原料,在实验室采用两段糠醛萃取组合工艺技术进行生产高芳烃含量橡胶增塑剂的研究。结果表明:采用两段糠醛萃取反序工艺可以得到满足GB/T 33322—2016《橡胶增塑剂芳香基矿物油》A1820要求的橡胶增塑剂产品,其收率占减三线馏分油的26.8%;工业装置实际运行验证了实验室研究结果,且得到了性质和收率略优于实验室数据的产品。
CNOOC SZ36-1 vacuum 3 rd line fraction was used as raw material to produce rubber plasticizer by using two stage furfural extractions in laboratory.The results showed that the reverse order process could produce the rubber plasticizer meeting the specification of A1820 according to the national standard GB/T 33322—2016 and the yield is 26.8%.The actual operation of the industrial unit verified the laboratory results.The properties and yield of industrial product are both slightly better than laboratory.
引文
[1]于恩强,付玉娥,马景光,等.国内环保轮胎橡胶油产品与市场现状[J].润滑油,2012,27(1):12-17
[2]付玉娥,于恩强,商希红,等.环保橡胶油的研究开发及工业化[J].润滑油,2011,26(5):7-11
[3]田义斌,张翠侦,马莉莉,等.环烷基减三线馏分油生产环保橡胶油工艺研究[J].石油炼制与化工,2017,48(6):69-73
[4]GB/T 33322—2016.橡胶增塑剂芳香基矿物油[S].2017-07-01
[5]辛秀婷,熊春珠,周勇,等.克拉玛依石化公司环保型橡胶填充油[J].橡胶科技市场,2009(17):20-23
[6]付玉娥,宫鑫,王云霞,等.环保型橡胶填充油类型及生产现状[J].齐鲁石油化工,2012,40(5):168-171
[7]孙井侠,黄鹤,刘海澄.轮胎用环境友好型橡胶填充油的研究开发[J].橡胶科技市场,2007(9):13-15
[8]孙井侠.芳烃油替代品的研发和应用展望[J].橡胶科技市场,2007(20):5-8
[9]王玉章,吴艳萍,施昌智,等.环保型芳烃橡胶填充油抽提工艺开发与工业应用[J].石油炼制与化工,2011,42(7):1-4