摘要
综述了国内外桥梁钢的发展。重点讨论了高强度桥梁钢焊缝微观组织、力学性能和耐蚀性以及焊后热处理对焊缝性能的影响。
The development of bridge steel in domestic and overseas. The microstructure,properties and corrosion resistance of high-strength bridge steel welding joint and the influence of heat treatment after welding on the weld performance.
引文
[1]陈伯鑫.中国焊接钢桥的发展[J].电焊机,2007,37(3):1-5.
[2]高宗余,方秦汉,卫军,等.中国铁路桥梁技术发展与展望[J].铁道工程学报,2007(1):55-59.
[3]王磊,高彩茹,王彦锋,等.我国桥梁钢的发展历程及展望[J].机械工程材料,2008(5):1-3.
[4]段兰,王春生.高性能钢桥在北美的研究及应用简介[J].建筑钢结构进展,2008,10(2):50-61.
[5]姚昌荣,李亚东,强士中,等.美国桥梁高性能钢的发展与应用[J].世界桥梁,2005(1):57-61.
[6]盛尔迈,李思明.美日用于桥梁结构的高性能钢材[J].上海建材,2004(4):19-21.
[7]王春生,段兰,袁卓亚,等.高性能钢在日本及欧洲的研发与应用[J].世界桥梁,2008(1):68-72.
[8]Chen Xizhang,Huang Yuming. Hot deformation behavior of HSLA steel Q690 and phase transformation during compression[J]. Journal of Alloys and Compounds,2015,619:564-571.
[9]Ma Tianyu,Hu Yifei,Liu Xiao,et al. Experimental investigation into high strength Q690 steel welded H-sections under combined compression and bending[J]. Journal of Constructional Steel Research,2018,144:119-134.
[10]Yu Baojun,Guan Xiaojun,Wang Lijun,et al. Hot deformation behavior and constitutive relationship of Q420qE steel[J].Journal of Central South University of Technology,2011,18(1):36-41.
[11]Wang Chunsheng,Duan Lan,Chen Y,et al. Flexural behavior and ductility of hybrid high performance steel I-girders[J].Journal of Constructional Steel Research,2016,125:1-14.
[12]Pan Y,Zhang Y,Tian Y,et al. Study on the ultimate bearing capacity of I-shaped beam made by high performance steel Q500qE[J]. China Railway Science,2011,32(3):16-20.
[13]陈尹泽,王立群,宋立伟,等. TMCP桥梁钢焊接接头组织性能研究[J].河南冶金,2017,25(2):8-9,25.
[14]于庆波. M/A岛对粒状贝氏体钢冲击韧性的影响[J].热加工工艺,2012,41(24):41-42.
[15]王正品,赵阳,王弘喆,等. M/A岛对T24钢焊接接头不完全淬火区组织性能影响[J].热力发电,2016,45(4):89-94.
[16]朱官朋,郭纯,姚润钢,等.低合金钢焊缝中针状铁素体的形成及影响因素[J].材料开发与应用,2014,29(03):87-93.
[17]贾坤宁,王海东,姜秋月,等.高强度桥梁钢焊接接头疲劳性能的研究[J].金属热处理,2009,34(4):48-51.
[18]Yu Qiming. Specimen's short fatigue crack fabrication test for Q420qE[C]//Information Engineering Research Institute,USA. Proceedings of 2013 2nd International Conference on Manufacture Engineering,Quality and Production System(ICMEQP 2013). USA:Information Engineering Research Institute,2013:3.
[19]贾坤宁,王海东,姜秋月,等.高强度桥梁钢焊接接头疲劳裂纹扩展速率的研究[J].热加工工艺,2010,39(17):4-7.
[20]Zong Liang,Shi Gang,Wang Yuanqing,et al. Experimental investigation on fatigue crack behavior of bridge steel Q345qD base metal and butt weld[J]. Materials and Design,2015,66:196-208.
[21]宗亮,施刚,王元清,等. Q345qD桥梁钢对接焊缝疲劳裂纹扩展性能试验研究[J].铁道科学与工程学报,2015,12(1):105-112.
[22]于美,王瑞阳,刘建华,等.模拟海洋环境中两种结构钢焊接接头腐蚀特性[J].北京航空航天大学学报,2013,39(8):1020-1025.
[23]Guo Jia,Shang Chengjia,Yang Shanwu,et al. Effect of carbon content on mechanical properties and weather resistance of high performance bridge steels[J]. Journal of Iron and Steel Research International,2009,16(6):63-69.
[24]王志奋,骆海贺,吴立新,等.晶粒尺寸对桥梁钢的耐腐蚀性能影响[J].物理测试,2011(S1):115-120.
[25]李琳,徐小连,艾芳芳,等.晶粒尺寸对桥梁耐候钢耐大气腐蚀性能的影响[J].腐蚀与防护,2013,34(11):1001-1004.
[26]黄元林,向学建,朱有利,等.超声冲击处理对Q370qE钢焊接接头耐腐蚀性能的影响[J].金属热处理,2012,37(11):24-27.
[27] Chen Xizhang, Huang Yuming, Lei Yucheng, et al.Microstructure and properties of 700MPa grade HSLA steel during high temperature deformation[J]. Journal of Alloys and Compounds,2015,631:225-231.
[28]刘立彪,张计谋,谭小斌,等.焊后热处理温度对Q420 R性能与组织的影响[J].世界有色金属,2017(23):234-235.