摘要
采用静电层层自组装技术将丝素(SF)与聚乙烯亚胺(PEI)复合制备的SF/PEI纳米纤维,随着自组装层数的增多,纤维直径变粗,表面变得不规整,且在一定的自组装层数内,复合纳米纤维膜对Cu2+的过滤效率不断增大.杂化Fe后,纤维表面变得更加凹凸不平,但对Cu2+的过滤效果显著改善.这对于制备新型、高效、无二次污染、低治理成本的替代或改进的重金属过滤材料提供了理论意义.
F/PEI composite Nano fiber membrane was made in this experiment by layer-layer electrostatic self-assembly technology,With the increasing in the number in self-assembly layer,the fiber diameter become larger,the surface become irregular,and in certain layer,the adsorption efficiency of Cu2+ increases.After the hybrid Fe,fiber surface become more uneven,but the adsorption efficiency improved significantly.This experiment provides theoretical significance for new,effective,no secondary pollution and low management cost alternative or improved heavy metal filter material.
引文
[1]唐圣奎,谢军军,熊杰.基于不同溶剂静电纺再生丝素蛋白组织工程支架的研究与进[J].中国组织工程研究与l临床康复,2008,12(45):8889-8892.
[2]安富强,高保娇,刘青.PEIP SiO 2复合材料对Zn 2+、Cd 2+的螯合吸附性能研究[J].化学通报,2006,3:201-206.
[3]Barhaters,Chong K L,Seeram R.Preparation and char-acterization of nanofibrous filtering media[J].Membr Sci,2006,283:209-218.
[4]Formhals A.Process and apparatus for preparing artifi-cial threads[P].US Patent:1975504,1934.
[5]居静霞,张幼珠,尹桂波.再生丝素纳米纤维的制备及其应用[J].丝绸,2004,7:41-43.
[6]张瑞华,孙红文.零价铁修复铬污染水体的实验研究[J].农业环境学学报,2004,23(6):11.