以磷酸镁钾水泥(MKPC)和硅灰作为固化剂,固化城市生活污泥。通过探究MKPC掺加量、污泥的含水率以及硅灰掺量等因素,研究了MKPC对污泥固化减量效果的影响规律。
Magnesium phosphate potassium cement( MKPC) and silica fume are used as curing agents to solidify urban sludge.The influence of MKPC on sludge solidification and reduction was studied by investigating factors such as the amount of MKPC added,the moisture content of sludge,and the content of silica fume.