摘要
CO_2+O_2地浸采铀工艺在我国砂岩型地浸采铀矿山逐渐得到应用。针对内蒙古某CO_2+O_2地浸采铀矿山水冶工艺运行中存在的较为严重的树脂板结问题,通过全面分析、实践,提出了板结树脂处理方案,缓解了树脂板结问题,进一步优化了工艺参数,对今后采用水冶回收工艺中解决树脂板结问题有积极的指导作用。
CO_2+O_2 in-situ leaching uranium has been gradually applied in sandstone deposit in our country.This article according to the serious resin hardening problems exist in the hydrometallurgy process of CO_2 + O_2 in-situ leaching uranium in Inner Mongolia,through comprehensive analysis,practice,put forward the cleaning method of hardening resin,not only alleviated the resin hardening problem,further optimization the project construction parameters,but also plays a guiding role in resin hardening of Hydrometallurgy process of CO_2+O_2 in-situ leaching uranium in our country.
引文
[1]张国建,王海峰,姜岩,等.美国碱法地浸采铀工艺技术概况[J].铀矿冶,2005,24(1):6-13.
    [2]田新军,沈红伟,陈雪莲,等.用二氧化碳减缓碱法地浸采铀中的化学沉淀堵塞[J].铀矿冶,2006,25(1):15-20.
    [3]杨解.铀矿水文地质基础[M].北京:原子能出版社,1988:133,142-143.
    [4]苏学斌,韩青涛,谭亚辉,等.新疆某CO_2地浸采铀试验研究[J].铀矿冶,2005,24(3):129-134.

© 2004-2018 中国地质图书馆版权所有 京ICP备05064691号 京公网安备11010802017129号

地址:北京市海淀区学院路29号 邮编:100083

电话:办公室:(+86 10)66554848;文献借阅、咨询服务、科技查新:66554700