摘要
采用中型固定床加氢装置考察了含氮化合物对柴油超深度加氢脱硫Ni-Mo-W型催化剂运行稳定性的影响。通过元素分析、N_2吸附-脱附、热重-质谱(TG-MS)联用、X射线光电子能谱(XPS)、高分辨透射电镜(TEM)等表征手段研究了催化剂失活的主要原因。实验结果表明:原料添加含氮化合物后,主要影响了催化剂的初活性,运转初期反应温度提高了7~10℃,但对催化剂的稳定性影响不大。根据催化剂失活原因的分析发现,原料添加含氮化合物前后,催化剂失活的主要原因均与其表面积炭的形成、孔体积的损失和边缘W比例的下降密切相关。
With using Ni-Mo-W/γ-Al_2O_3 catalyst,effect of nitrogen compounds on the running stability of ultra-deep hydro-desulfurization diesel catalyst was studied on a pilot plant unit.The reasons of catalyst deactivation were investigated by different characterization techniques which included elemental analysis,nitrogen adsorption-desorption,thermal gravity-mass spectrometry(TG-MS),X-ray photoelectron spectroscopy(XPS)and high resolution transmission electron microscopy(TEM).Experimental results suggest that nitrogen compounds mainly impact on catalyst initial activity,and lead to initial reaction temperature 7 to 10 ℃ higher.However,nitrogen compounds have little impact on catalyst stability.With/without nitrogen compounds adding into the feedstocks,the main reasons of catalyst deactivation are all mainly related to the surface coking,loss of pore volume and decrease of edge tungsten.
引文
[1]LANDAU M V.Deep hydrotreating of middle distillates from crude and shale oils[J].Catalysis Today,1997,36(4):393-429.
[2]TORRISI S,DICAMILLO D,STREET R,et al.Proven best practices for ULSD production[C]//San Antonio:National Petrochemical&Refiners Association,2002.
[3]王丹,宋金鹤,韩志波,等.柴油加氢精制催化剂的开发及工业应用[J].石油化工,2017,46(2):241-247.(WANG Dan,SONG Jinhe,HAN Zhibo,et al.Development and commercial application of diesel hydrotreating catalyst[J].Petrochemical Technology,2017,46(2):241-247.)
[4]FURIMSKY E,MASSOTH F E.Deactivation of hydroprocessing catalysts[J].Catalysis Today,1999,52(4):381-495.
[5]FURIMSKY E,MASSOTH F E.Hydrodenitrogenation of petroleum[J].Catalysis Reviews,2005,47(3):297-489.
[6]BREYSSE M,FURIMSKY E,KASZTELAN S,et al.Hydrogen activation by transition metal sulfides[J].Catalysis Reviews,2002,44(4):651-735.
[7]魏计春,齐邦峰,张会成.催化柴油中含氮化合物的研究[J].化工科技,2010,18(1):60-63.(WEI Jichun,QI Bangfeng,ZHANG Huicheng.The research of nitrogen compounds in diesel oil[J].Science&Technology in Chemical Industry,2010,18(1):60-63.)
[8]YOSHIMURA Y,SATO T,SHIMADA H,et al.Oxidative regeneration of spent molybdate and tungstate hydrotreating catalysts[J].Energy&Fuels,1994,8(2):435-445.
[9]GURICHARD B,ROY-AUBERGER M,DEVERS E,et al.Characterization of aged hydrotreating catalysts Part I:Coke depositions,study on the chemical nature and environment[J].Applied Catalysis A:General,2009,367(1/2):1-8.
[10]邱丽美,齐和日玛,刘清河,等.X射线光电子能谱法研究加氢脱硫催化剂中活性元素的化学态[J].石油学报(石油加工),2011,27(4):638-642.(QIU Limei,QI Herima,LIU Qinghe,et al.Investigation of chemical states for hydrodesulfurization catalysts by using X-Ray photoelectron spectroscopy[J].Acta Petrolei Sinica(Petroleum Processing Section),2011,27(4):638-642.)
[11]QIU L,XU G.Peak overlaps and corresponding solutions in the X-ray photoelectron spectroscopic study of hydrodesulfurization catalysts[J].Applied Surface Science,2010,256(11):3413-3417.
[12]HAN W,YUAN P,FAN Y,et al.Preparation of supported hydrodesulfurization catalysts with enhanced performance using Mo-based inorganic-organic hybrid nanocrystals as a superior precursor[J].Journal of Materials Chemistry,2012,22(48):25340-25353.
[13]HENSEN E J M,KOOYMAN P J,van DER MEER Y,et al.The relation between morphology and hydrotreating activity for supported MoS2 particles[J].Journal of Catalysis,2001,199(2):224-235.
[14]张妍茹.加氢催化剂活性金属高效再分散的研究[D].北京:石油化工科学研究院,2016.
[15]邵志才,高晓冬,李皓光,等.氮化物对柴油深度和超深度加氢脱硫的影响Ⅰ氮化物含量的影响[J].石油学报(石油加工),2006,22(4):12-18.(SHAO Zhicai,GAO Xiaodong,LI Haoguang,et al.Effect of nitrogencontaining compounds on deep and ultra deep HDS for diesel oil I Effect of the content of nitrogen-containing compounds[J].Acta Petrolei Sinica(Petroleum Processing Section),2006,22(4):12-18.)
[16]刘法.柴油馏分超深度加氢脱硫动力学模型研究[D].北京:石油化工科学研究院,2006.
[17]ANCHEYTA J,ANGELES M J,MACIAS M J,et al.Changes in apparent reaction order and activation energy in the hydrodesulfurization of real feedstocks[J].Energy&Fuels,2002,16(1):189-193.
[18]葛泮珠,丁石,张乐,等.氮化物对Ni-Mo-W和Co-Mo型催化剂超深度加氢脱硫反应的影响[J].石油化工,2017,46(2):171-176.(GE Panzhu,DING Shi,ZHANG Le,et al.Effect of nitrogen-compounds on ultra-deep HDS for diesel oil on Ni-Mo-W/Al2O3 and Co-Mo/Al2O3catalysts[J].Petrochemical Technology,2017,46(2):171-176.)
[19]MARAFI A,STAINSLAUS A,HAUSER A,et al.An investigation of the deactivation behavior of industrial Mo/Al2O3and Ni-Mo/Al2O3 catalysts in hydrotreating Kuwait atmospheric residue[J].Petroleum Science and Technology,2005,23:385-408.
[20]MATSUSHITA K,HAUSER A,MARAFI A,et al.Initial coke deposition on hydrotreating catalysts Part 1Changes in coke properties as a function of time on stream[J].Fuel,2004,83(7/8):1031-1038.
[21]DONG D,JEONG S,MASSOTH F E.Effect of nitrogen compounds on deactivation of hydrotreating catalysts by coke[J].Catalysis Today,1997,37(3):267-275.
[22]陈士锋,陈海,杨朝合.渣油加氢转化过程结焦催化剂的表征[J].石油学报(石油加工),2002,18(3):8-13.(CHEN Shifeng,CHEN Hai,YANG Chaohe.Characterization of coked catalysts for residual hydroconversion process[J].Acta Petrolei Sinica(Petroleum Processing Section),2002,18(3):8-13.)
[23]SAHOO S K,RAY S S,SINGH I D.Structural characterization of coke on spent hydroprocessing catalysts used for processing of vacuum gas oil[J].Applied Catalysis A:General,2004,278(1):83-91.
[24]CALLEJAS M A,INEZ M T M,BLASCO T,et al.Coke characterisation in aged residue hydrotreating catalysts by solid-state 13 C-NMR spectroscopy and temperature-programmed oxidation[J].Applied Catalysis A:General,2001,218:181-188.
[25]GE P,ZHANG L,DING S,et al.Correlation of deactivation of Ni-Mo-W/Al2O3 during ultra-low-sulfur diesel production with surface carbon species[J].China Petroleum Processing&Petrochemical Technology,2017,19(2):1-7.
[26]van DOOM J,MOULIJN J A,DJEGA-MARIADASSOU G.High-resolution electron microscopy of spent Ni-Mo/Al2O3 hydrotreating catalysts[J].Applied Catalysis,1990,63(1):77-90.
[27]DIEZ F,GATES B C,MILLER J T,et al.Deactivation of a Ni-Mo/γ-Al2O3 catalyst:Influence of coke on the hydroprocessing activity[J].Industrial&Engineering Chemistry Research,1990,29(10):1999-2004.