Accelerated corrosion of 2205 duplex stainless steel caused by marine aerobic Pseudomonas aeruginosa biofilm
文摘
<p id="p0005">LPR and EIS showed that P. aeruginosa reduced the corrosion resistance of 2205 DSS.p>
<p id="p0010">The largest pit depth on 2205 DSS was 4.9 μm after 14 days incubation in sterile medium.p>
<p id="p0015">The largest pit depth on 2205 DSS was 14 μm after 14 days incubation with P. aeruginosa.p>
<p id="p0020">The accelerated pitting was due to the formation of CrO3 and CrN by P. aeruginosa.p>