Effects of building orientation and heat treatment on fatigue behavior of selective laser melted 17-4 PH stainless steel
详细信息    查看全文
文摘

Fatigue behavior of SLM 17-4 PH SS and its dependence to microstructure and defects.

Effects of building orientation and heat treatment on fatigue behavior.

Fracture surface traits and failure mechanisms of SLM 17-4 PH SS specimens.

Some important factors for optimizing additive manufacturing process parameters.