Sinusoidal perturbed Al foil was prepared by single-point diamond turning.
•
Perturbed Al foil was measured by surface profiler and white light interferometer.
•
Perturbed Al foil and CH layer adhered with each other via a hot-press process.
•
Parameters and cross-section of the CH–Al perturbation target was characterized.