The hot deformation behavior and microstructure of AZ31 and AZ61 alloys processed by the hot-rolled technique were investigated over a strain rate range from 1脳10鈭? to 1脳10鈭? s鈭? and temperatures ranging from 350 to 500 掳C. Alloys were manufactured by melting and casting, and then hot-rolled at two temperatures of 350 and 450 掳C. Tensile test revealed elongations of over 300% in the two alloys. The highest elongation value of 321% at a strain rate of 3脳10鈭? s鈭? was achieved in the AZ61 alloy with a hot-rolling temperature of 350 掳C. The hot tensile tests showed that there are some differences in ductility between the AZ31 and AZ61 alloys with the same rolling process specifically at low strain rates. A small enhancement in ductility is found using a lower temperature for hot-rolling at 350 掳C compared to 450 掳C due to improved grain refinement. It is suggested that the dominant deformation mechanism was glide controlled dislocation creep based on the stress and grain size exponent, and activation energy.
NGLC 2004-2010.National Geological Library of China All Rights Reserved.
Add:29 Xueyuan Rd,Haidian District,Beijing,PRC. Mail Add: 8324 mailbox 100083
For exchange or info please contact us via email.