LiVPO4F/C cathode was synthesized by a fast chemical reduction method.
Low toxicity NH4VO3 was reduced by oxalic acid at 60 °C in short time.
Polyvinylidene fluoride was used as carbon source with ultrasonic dispersion.
The binding energy peaks corroborate that V in NH4VO3 was effective reduced.
LiVPO4F/C cathode prepared possesses excellent performances.