Heat release rate of Mg alloys increase with Mg content.
•
FPI of ZE10 is 18% lower than AZ31 and 17% lower than WE43.
•
Activation energy of ZE10 is 13.7% and 10.1% higher than AZ31 and WE43.
•
The sharp oxidation in TG tests occurs at a certain extent of conversion.