Degradation of oxygen reduction reaction kinetics in porous La0.6Sr0.4Co0.2Fe0.8O3-δ cathodes due to aging-induced changes in surface chemistry
详细信息    查看全文
文摘
Surface La- and Sr-enrichment induced by aging LSCFO cathodes at 800 °C for 50 h. Cation redistribution can extend up to ∼400 nm depth under the LSCFO surface. Surface chemical changes detected by high resolution STEM/EDS maps at cathode pores. Oxygen exchange at LSCFO/gas interface hampered by surface chemistry modification. Oxygen ion conductivity remains constant upon aging according to impedance analysis.