A multistep sintering protocol is proposed to synthesize cubic phase Li garnets.

class="label">•

Cubic garnet, once formed, remains stable even after keeping at 1200 °C for 24 h.

class="label">•

The as-prepared pellets exhibit δRT of 4.5 × 10−4 S cm−1.