A Fe-30Mn-3Si-3Al TWIP steel did not show fatigue crack non-propagation at the fatigue limit.

A Fe-23Mn-0.5C TWIP steel showed fatigue crack non-propagation.

The crack non-propagation of the Fe-Mn-C steel probably because of dynamic strain aging.

The dynamic strain aging seems to assist fatigue crack initiation.