Silico-Aluminous Bottom Ash was successfully recycled in kiln feed.
•
Raw meals particle size was reduced with the increment of SABA addition.
•
Clinker main mineralogical phases weren’t negatively affected by SABA presence.
•
All syntheses satisfied the requirements for the strength class 52.5 as per standard EN 197-1.