SrAlxFe12-xO19 (x = 0–4) were synthesized via a mechanochemical activation.

class="label">•

Deterioration of magnetic properties by milling depends on Al content.

class="label">•

A subsequent annealing treatment in NaCl melt at 1000 °C promotes recrystallization.

class="label">•

Annealing treatment in NaCl melt at 1000 °C increases magnetic properties.

class="label">•

Coercivity is explained by single domain particles and correlated to initial curve.