The maximum aO2 is found at the YSZ/CGO10 interface of a bi-layer electrolyte SOEC.

Operating cyclically between SOFC and SOEC mode can mitigate degradation.

Increasing n- to p-type electrolyte conductivity reduces volume exposed to high aO2.

Reversal of a43602eb93fef67efe6847145821dd9e" title="Click to view the MathML source">iion and aO2 distribution can occur in heterogeneously degraded cells.