Hazard waste from asbestos fiber production with high levels of lizardite and brucite was assessed.
ass="label">•
Mg and Fe extraction was assessed using DoE applying Taguchi Method.
ass="label">•
Highest Mg and Fe extraction were reached under mild process condition.
ass="label">•
Acid excess have not much influence on leaching step.
ass="label">•
High dissolution of serpentines was reached during the first 30 min of reaction.